Stainless steels Manwal nga electrode E2594-16 Soldering makings
Aplikasyon
Kini angay alang sa welding sa 25% Cr duplex stainless steel sa offshore nga lana, natural nga gas ug petrochemical nga mga industriya. Pananglitan, 0022CrNi7Mo4N, 03Cr25Ni6Mo3Cu2N, UNS 32550 (Alloy255) UNS S32750.
Lawas sa sertipikasyon: BV, CCS, LR, NK
KEMIKAL NGA COMPONET:
HALOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | N | Cu | |
GB/T MGA LAGDA | 0.04 | 0.5-2.0 | 1.00 | 24.0-27.0 | 8.0-10.5 | 3.4-4.5 | 0.04 | 0.03 | 0.20-0.30 | 0.75 | |
MGA LAGDA SA AWS | 0.04 | 0.5-2.0 | 1.00 | 24.0-27.0 | 8.0-10.5 | 3.4-4.5 | 0.04 | 0.03 | 0.20-0.30 | 0.75 | |
Ehemplo nga BILI | 0.021 | 0.85 | 0.74 | 25.2 | 9.1 | 4.05 | 0.021 | 0.005 | 0.25 | 0.05 |
MEKANIKAL NGA PROPERTY:
PROPERTY | KUSOG SA ANI(MPa) | PAGPAPADAYON NGA KUSOG(MPa) | IMAPACT VALUE J/℃ | ELONGATION(%) | ||||
GB/T MGA LAGDA | - | 760 | - | 13 | ||||
MGA LAGDA SA AWS | - | 760 | - | 15 | ||||
Ehemplo nga BILI | - | 915 | - | 22.5 |
GIREKOMENDADONG MGA PARAMETER SA WELDING:
DIAMETERS ESPESPIKASYON(mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||
KURYENTE (Amp) | H/W | 50-75 | 70-95 | 80-120 | 110-160 | 160-190 | ||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |
Titanium-calcium two-phase stainless steel kamot electrode, ang nag-unang component mao ang 25.5Cr-10Ni-4Mo-0.25N;
Ang weld metal mao ang austenitic ferrite biphase structure, nga adunay taas nga kusog, maayo nga pitting ug stress corrosion cracking resistance, maayo kaayo nga thermal crack resistance, PREN (pitting resistance equivalent) ≥40.
Ningbo Honest Metal Materials Co, Ltd. mao ang usa ka internasyonal nga welding propesyonal nga kompanya sa sulod sa independenteng panukiduki ug kalamboan, produksyon, pagbaligya ug pagdumala. Natukod kini kaniadtong 2020.
85000 m3 Dako kaayo nga ethane Ethylene Carrier (VLEC)
Harbin Electric - Sanmen, Haiyang MSR
Polypropylene reactor
KEMIKAL NGA COMPONET:
HALOY(wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | N | Cu | |
GB/T MGA LAGDA | 0.04 | 0.5-2.0 | 1.00 | 24.0-27.0 | 8.0-10.5 | 3.4-4.5 | 0.04 | 0.03 | 0.20-0.30 | 0.75 | |
MGA LAGDA SA AWS | 0.04 | 0.5-2.0 | 1.00 | 24.0-27.0 | 8.0-10.5 | 3.4-4.5 | 0.04 | 0.03 | 0.20-0.30 | 0.75 | |
Ehemplo nga BILI | 0.021 | 0.85 | 0.74 | 25.2 | 9.1 | 4.05 | 0.021 | 0.005 | 0.25 | 0.05 |
MEKANIKAL NGA PROPERTY:
PROPERTY | KUSOG SA ANI(MPa) | PAGPAPADAYON NGA KUSOG(MPa) | IMAPACT VALUE J/℃ | ELONGATION(%) | ||||
GB/T MGA LAGDA | - | 760 | - | 13 | ||||
MGA LAGDA SA AWS | - | 760 | - | 15 | ||||
Ehemplo nga BILI | - | 915 | - | 22.5 |
GIREKOMENDADONG MGA PARAMETER SA WELDING:
DIAMETERS ESPESPIKASYON(mm) | 2.0*250 | 2.6*300 | 3.2*350 | 4.0*350 | 5.0*350 | |||||
KURYENTE (Amp) | H/W | 50-75 | 70-95 | 80-120 | 110-160 | 160-190 | ||||
O/W | 20-50 | 45-80 | 70-110 | 90-135 | - |